Productnummer | Technische specificaties | ||||
Vaste koolstof (≥%) | Vluchtig(≤%) | As(≤%) | Vocht (≤%) | Blijft op zeef (%) | |
MR50-80 MR80-80 MR100-80
MR120-80 MR150-80 |
80.00 | 2.70-3.00 | 17.00-17.30 | 1.00 | ≥80.00 |
MRG100-80 MRG200-80
MRG325-80 MRG500-80 |
≤20.00 | ||||
MR50-83 MR80-83 MR100-83
MR120-83 MR150-83 |
83 | 2.60-3.00 | 14.00-14.40 | 1.00 | ≥80.00 |
MRG100-83 MRG200-83
MRG325-83 MRG500-83 |
≤20.00 | ||||
MR50-85 MR80-85 MR100-85
MR120-83 MR150-85 |
85 | 2.30-2.50 | 12.50-12.70 | 1.00 | ≥80.00 |
MRG100-85 MRG200-85
MRG325-85 MRG500-85 |
≤20.00 | ||||
|
2.30-2.50 | 11.50-11.70 | 1.00 | ≥80.00 | |
|
≤20.00 | ||||
|
87 | 2.20-2.5 | 10.50-10.80 | 1.00 | ≥80.00 |
|
≤20.00 | ||||
|
88 | 1.80-2.00 | 10.00-10.20 | 1.00 | ≥80.00 |
|
≤20.00 | ||||
|
89 | 1.80-2.00 | 9.00-9.20 | 1.00 | ≥80.00 |
|
≤20.00 | ||||
|
90 | 1.80-2.00 | 8.00-8.20 | 1.00 | ≥80.00 |
|
≤20.00 | ||||
|
91 | 1.40-1.60 | 7.40-7.60 | 1.00 | ≥80.00 |
|
≤20.00 | ||||
|
92 | 1.35-1.55 | 6.45-6.65 | 1.00 | ≥80.00 |
|
≤20.00 | ||||
|
93 | 1.30-1.50 | 5.50-5.70 | 1.00 | ≥80.00 |
|
≤20.00 |
koolstofgehalte | 85-99.4% | 85-99.5% | 99.80% |
PH: | 3-7 | 3-7 | 3-7 |
vluchtigheid: | ≤20% | ≤18% | ≤20% |
vocht% | ≤1% | ≤1% | ≤0.8% |
S% | ≤2.50 | ≤2.50 | ≤2.00 |
De begintemperatuur | 190-200ºC | 220 °C. | 200°C. |
32 mesh | Expansietemperatuur:≥750ºC inflatiepercentage: 250-550(ml/g) | ||
50 mesh | Expansietemperatuur:≥750ºC inflatiepercentage: 250-450(ml/g) | ||
80 mesh | Expansietemperatuur:≥750ºC inflatiepercentage: 200-350(ml/g) | ||
150 mesh | Expansietemperatuur:≥750ºC inflatiepercentage: 100-200(ml/g) | ||
Toepassingsveld: | Vlamvertragend polyurethaan schuimen, EPS, brandafdichting, PU, XPS | ||
Stalen metalen beschermresidu | |||
Brandvertragend lakadditief. | |||
Natuurlijk vlokgrafiet |